Dear MEMS Group,

we used the RIE process for etching SiN and achieved with a SF6 flow of
100sccm, a pressure of 200mT and a RF-Power of 50W a etchrate of approximately
1000A/min.

Does anyone used this process and obtained a significantly lower etchrate
(maybe 100A/min) with a uniform surface? Which parameters did you use?

Thank you very much for your help,

Michael Traxler and Matthias Meyer
Graduate Students
University of Washington
Department of Physics


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation