Siddharth,

There are several MEMS companies that may provide aligned wafer bond service. Be
prepared ... Unless they have a microscope that will allow for ISA (inner
substrate alignment)  at lease one of your substrates will require a pattern on
the backside that is referenced to the opposite (bond) side.

You may want to contact IntelliSense    16 Upton Drive Wilmington, MA 01887
978-988-8000 www.intellis.com

Standard MEMS  80 Arkay Drive Happauge, NY 11788
516 435-6381 www.smsc.com

Regards,







Joe Brown
MEMS
Karl Suss America
[email protected]
802-244-5181X250
802-244-5103 Fax


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
MEMS Technology Review
University Wafer