Re: Negative photoresist
1999-09-08
CLIF HAMEL
Re: Negative photoresist
CLIF HAMEL
1999-09-08
Do you have a positive acting resist you have used?  If so, then you can reverse
it using the image reversal method.  You can mix imidazole with the resist or
you can use ammonia vapors to reverse it after image exposure.  I will provide
more details if you are interested.

Clif

>>> SILLON Nicolas  09/07 4:34 AM >>>

Hello,
I'm looking for a high resolution negative (or reversible) photoresist for
gold electroplating. I tried AZ 5214 but it doesn't seem to be compatible
with gold plating.
Any advice  is appreciated.
Thank You.

SILLON Nicolas
CEA / Leti
DMITEC / SIA / ES
17 rue des Martyrs
38 054 GRENOBLE Cedex 9
Tel:   (33) 4 76 88 36 01
Fax:  (33) 4 76 88 94 56


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Addison Engineering