A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Glass Etching
Glass Etching
1999-09-22
Weijie Wang
Glass Etching
Weijie Wang
1999-09-22
Hi,

I am trying to etch grooves on glass (Corning 7740) using BOE as etchant,
after 30 Min. etching, seems nothing happened. Does anyone know what's
reason for it?

Thank you in advance.

Weijie Wang
[email protected]