MEMSnet Home: MEMS-Talk: Re: KOH etch station for 6"
Re: KOH etch station for 6"
1998-12-24
[email protected]
Re: KOH etch station for 6"
[email protected]
1998-12-24
From:  Robert Antaki@MITEL on 12/23/98 07:44 PM
Try Lufran they make micro-electronics etch baths

www.lufran.com
or
1-800-726-5934

sincerely,
Robert A.