Dear Deena,

I found these values in the book "Handbook on Physical Properties
of Ge, Si, GaAs and InP" by A. Dargys and J. Kundrotas.

specific heat of GaAs: 0.33 J/(g.K)
Thermal conductivity: 0.58 W/(cm.K)

both are values at room temperature.

Debjani

Research Scholar (Semiconductor Group)
Department of Physics                 Ph: (080)309-2316
Indian Institute of Science           Fax:(080)334-1683
Bangalore - 560012


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation