Hi,
I'm trying to solve a thermal-mismatch problem between two parts,
consisting of Pyrex glass and aluminium-ceramik(al2o3) by bonding them
with an elastic adhesive.
Could someone give me hints on which adhesive would be suitable?
Thank you in advance.

Sincerly, W.Brueck