MEMSnet Home: MEMS-Talk: chromium lift-off from pyrex glass, etching in 1:1 HF
chromium lift-off from pyrex glass, etching in 1:1 HF
1999-01-13
arvind tiwari
chromium lift-off from pyrex glass, etching in 1:1 HF
arvind tiwari
1999-01-13
I'm interested in getting holes etched in 7740 pyrex glass.With Cr
deposition using magnetron sputtering, I find that Cr film lifts off
after one or one and half hour of etching in 1:1 HF.

ARVIND
CARE,IITD
INDIA
e-mail add: [email protected]

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
The Branford Group
Addison Engineering