        Dear colleagues,

        I am interested to apply a metal layer (CrAu for instance) in an array
of
V-grooves anisotropically etched in (100) Si. My question is the following:
        Are there any troubles regarding the metal deposition on the bottom of
the
V-grooves? If yes, how can I deal with those troubles?
        (the V-grooves are 70 microns wide and 30 microns deep)
        Best regards
        Vlad Badilita
Vlad Badilita - dipl. phys.
Multidisciplinary Research Dpt.
Micromachined Structures, Microwave Devices and Circuits Lab.
National Institute for Research and Development in Microtechnologies
                IMT - Bucharest
P.O. Box 38-150, Bucharest 72225, Romania
Fax: +40-1-230.75.19, +40-1-411.46.61
Web page: http://www.imt.ro


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation