My understanding is that Linotronic now makes printers capable of
printing on film to over 4000 dpi.  This would be about 6 micron dot
size.  However, 2540 dpi works out to 10 micron dot size, so if the
linotronic printer did not give you that quality of result you may want
to check other aspects of the system (i.e., does your program really
generate accurate data in the print file, and is the printer in good
condition?).

Thor Osborn, Ph.D.
Manager, MEMS Processing
Microvision, Inc.
2203 Airport Way South, Suite 100
Seattle, Washington 98134

TEL.    (206) 623-7055
FAX     (206) 467-8120


-----Original Message-----
From: John R Lodmell [mailto:[email protected]]
Sent: Thursday, February 04, 1999 10:38 AM
To: [email protected]
Subject: Better resolution for desktop publishing masks


        I have recently used a commercial printer to make a mask on
printer's
film.  He used a Linotronic printer with 2540 dpi.  The mask gave us
about 25
micron resolution, which I understand is pretty typical.
        I would really like about 10 micron resolution, but our
photolithography system does not have reduction capability (only 1:1).
Does
anyone know how to get closer to 10 microns?  Try to find higher dpi
capabilities?  Commercially available reduction to make a new mask from
the
existing mask?
        Any suggestions would be appreciated.

John Lodmell
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.