MEMSnet Home: MEMS-Talk: 8-inch silicon wafer processing needed!
8-inch silicon wafer processing needed!
1999-02-23
[email protected]
8-inch silicon wafer processing needed!
[email protected]
1999-02-23
     Hello everyone,

     Thanks to all for responding to my previous inquiries regarding
     ion milling. Before addressing that issue, however, I have a
     much more fundamental problem to solve. I'm currently dealing
     with 8-inch silicon wafers. Does anyone know of any foundrys out
     there willing to do process development work on 8-inch silicon
     wafers? I have an immediate need to characterize a fairly
     straight-forward process on 5-10 wafers. The process involves a spin-
     coating of a polyimide, metallization and passivation.

     Thanks for your input,

     Avinash Kane
     Raytheon Systems Company
     Fullerton, California
     (714) 446-2218
     [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics