A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: HMDS on metals
Re: HMDS on metals
1999-02-19
Shekhar Bhansali
1999-02-19
Michel Rosa
1999-02-22
Uthara Srinivasan
Re: HMDS on metals
Michel Rosa
1999-02-19
Todd -

Generally I use HMDS on SiO2 or nitride layers, Cleaned cilison or metal
layers should probably not require such coatings before PR applications,.

Regards,

Mike Rosa.

At 12:48 AM 2/16/99 PST, you wrote:
>Is HMDS useful as a resist adhesion promoter on substrates other than
>silicon? We use HMDS before applying resist to a gold coated wafer and I
>was wondering if this would have any benefit on gold-resist adhesion.
>
>Thanks,
>
>
>Todd
>
>
>
>

Xerox PARC
3333 Coyote Hill Rd,
Palo Alto. USA. 94304.

Ph : (650) 812-4162


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing