MEMSnet Home: MEMS-Talk: re:SiO2 deposition
re:SiO2 deposition
1999-02-22
[email protected]
re:SiO2 deposition
[email protected]
1999-02-22
Hi Robert

Have you considered Oxford Instruments DP80 or DP800 systems?  These are
plasma enhanced chemical vapour deposition systems, either running at
13.56MHz or using mixed frequency (to achieve stress control).  Try the web
site at http://www.oxfordplasma.com for your nearest agent or company site.
***********************************************
Plasma Technology, Oxford Instruments
North End, Yatton
Bristol, BS49 4AP, England
Tel: +44 (0)1934 833851 Fax: +44 (0)1934 834918
URL http://www.oxfordplasma.com/
***********************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Tanner EDA by Mentor Graphics
MEMStaff Inc.