Tolfree, DWL (Dave)
RE: Sputtered films vs Evaporated films
Tolfree, DWL (Dave)
1999-02-22
The general answer to your question is YES, but its very dependent on
process conditions and substrates

D Tolfree
FFNW

-----Original Message-----
From: Sung Jin [mailto:[email protected]]
Sent: 20 February 1999 2:56 AM
To: [email protected]
Subject: Sputtered films vs Evaporated films


Do sputtered films have in general higher stress levels than evaporated
films?

I am interested in general trends between the two modes of deposition.

Thank you.

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering