     Dear colleagues,

     I am interested in measuring the adhesion strength of epoxy on the
     Polymide (passivation layer on Si chip).

     Is there any big difference if the Polymide is sprayed on a substitute
     material instead of Si chip, for example steel so that fixtures can be
     made more easily?

     Thanks for your comments and suggestions

     Wang Hongbin

     STMicroelectronics


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group
Tanner EDA by Mentor Graphics