EDP etch rate ratios
1999-03-11
Steve G Forgrieve
EDP etch rate ratios
Steve G Forgrieve
1999-03-11
I am using either silicon dioxide or silicon nitride as a masking material
for an EDP etch. I plan to use EDP type"B" (ethylenediamine : pyrocatechol
: water ; 75ml : 12g : 25ml). My problem is I cannot find etch rate ratios
for the masking materials and the silicon<100>. I need to etch right
through a 380 micron wafer. Also, is type B EDP the best to minimize mask
under etch?
                        Thanks

PS. Thanks alot to those who helped with my Boron etch stop problem

Steve Forgrieve
Department of Electrical Engineering
The University of Edinburgh
King's Buildings
Mayfield Rd
Edinburgh EH9 3JL
(Int +44) 131 650 5665 (enquiries)
email: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.