MEMSnet Home: MEMS-Talk: Re: (111)
Re: (111)
1999-03-11
Jonathan Bernstein
1999-03-23
Fabio Coccetti
Re: (111)
Jonathan Bernstein
1999-03-11
The 111 planes are the slow etch planes:  it will not etch fast.
If you start with an unpolished wafer you will see a field of nice triangles,
reflecting the crystal symmetry.





At 10:45 AM 3/8/99 -0600, you wrote:
>If you have a Si wafer that is cut paraller to (111) plane.
>Has anyone done any etching on the wafer and can tell me
>what would be the ecth rate and the grove corner shapes under the mask after
>etching.
>
>
>
>I would apreaciate your response.
>
>email    [email protected]
>Fax      (817) 272-5010
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation