Hi,

I used ANSYS for simulations of the dynamic behaviour of piezoelectric
ceramic multilayer capacitors. It worked fine, we had good agreements with
our measurements.
But you have to build a volume FEM-model, and you have to be careful with
the ratio of your geometrics.

Try http:\\www.ansys.com for more information about ANSYS

I think there is another FEM-program which can handle piezoelectric
problems: ATILA from cedrat in grenoble.

Try http:\\www.cedrat-grenoble.fr, but I never worked with ATILA.

Greetings,
Timm Leuerer



**************************************************
* Timm Leuerer                                   *
* Institut fuer Werkstoffe der Elektrotechnik    *
* Lehrstuhl 1                                      *
* Sommerfeldstr. 24                              *
* RWTH-Aachen                                *
* 52056 Aachen                              *
* Germany                                        *
* Tel: ++49 / (0)241 / 80-7836                   *
* Fax: ++49 / (0)241 / 8888-392                  *
* [email protected]                     *
**************************************************


> -----Ursprüngliche Nachricht-----
> Von:  [email protected] [SMTP:[email protected]]
> Gesendet am:  Montag, 8. März 1999 15:08
> An:   [email protected]
> Betreff:      micro-manipulator with flexible beam
>
> Hi mems community !
>
> I'm working on the design of a micro-manipulator using adhesion forces
> with a gold coated monocrystal silicon cantilever (600x140x10 microns),
> attached to a piezzo accelerator on one end and free on the other. We've
> got problems on describing with precision the dynamic behavior of the beam
> (elastic, of course). We are currently trying somr finite elements
> software (abaqus) but they are  not friendly on dynamic. Any information
> or referance will be welcome... Thanx
>
> Sinan HALIYO
> LABORATOIRE DE ROBOTIQUE DE PARIS - Universite Paris 6
> [email protected]
> (33) 1 39 25 49 74
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review