MEMSnet Home: MEMS-Talk: Re: SiO2 Wet etch rate?
Re: SiO2 Wet etch rate?
1999-03-15
Kirthi Roberts
1999-03-15
Amit Shiwalkar
1999-03-16
Andrezej Prochaska
Re: SiO2 Wet etch rate?
Andrezej Prochaska
1999-03-16
Etch rate of SiO2 in Buffered HF is about 960A/min.
Etch rate of SiO2 in 1:10 HF is about 360A/min
Etch rate of SiO2 in KOH depends on temperature and solution contents. I don't
know what is the etch rate in 20:80 solution, but in 40:60 solution at 80C the
etch rate is about 55A/min.

Best regards,

Andrzej Prochaska


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing