MEMSnet Home: MEMS-Talk: RE: Looking for single side wet etching tools
RE: Looking for single side wet etching tools
1999-03-23
Zhou Wen Zhan
RE: Looking for single side wet etching tools
Zhou Wen Zhan
1999-03-23
You can try the SEZ backside etch system
The whole name of the company is Semiconductor Equipment und Zubehor AG, it
is in german
the address is:
                        Draubodenweg 29
                        A-9500 Villach
                        Phone 43/4242/204-0
                        Fax 43/4242/204-21
> ----------
> From:
> [email protected][SMTP:[email protected]
> .sextant.thomson-csf.com]
> Reply To:
> [email protected];[email protected]
> Sent:         12 March 1999 20:54
> To:   [email protected]
> Subject:      Looking for single side wet etching tools
>
> Dear MEMS community,
>
> We are currently looking for tools for silicon wet etching of 4" wafer in
> KOH with a proteection of one (active) side of the wafer.
>
> We need a highly reliable mechanical tool for our production line, with
> very low induced mechanical stress.
>
> Does anyone know a qualified supplier for such a tool?
>
> Regards
>
> Olivier LEFORT
> Microsensor design manager
> Sensor Unit
> SEXTANT Avionique
> Phone : 33 4 75 79 85 19
> Fax : 33 4 75 79 86 06
> [email protected]
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
MEMS Technology Review