Re: Etching Teflon
[email protected]
1999-03-23
We are doing some plasma etching of PTFE materials here at Trion Tech. Usually
thin layers and conditions of the reactors are approximate to what is used for
etching various oxides of silicon ie CF4, CHF3, ect.  Bob Henderson
602-968-8818


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics
Addison Engineering