A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: Pyralene C and Biocompatible materials needed
RE: Pyralene C and Biocompatible materials needed
1999-03-23
Karl Cazzini
1999-03-24
Thor Osborn
1999-03-24
Dr. Mark W. Lund
1999-03-23
Karl Cazzini
1999-03-24
Dr. Mark W. Lund
RE: Pyralene C and Biocompatible materials needed
Karl Cazzini
1999-03-23
See inset answers to some of your questions.

-----Original Message-----
From: [email protected] [mailto:[email protected]]On Behalf Of Sung Jin
Sent: Thursday, March 18, 1999 7:05 AM
To: [email protected]
Subject: Pyralene C and Biocompatible materials needed


Dear MEMS community,

I am looking for a biocompatible material, which is deposited easily,
by spin-coating for instance, and offers good durability for
microfluidic devices.

1. Could anyone tell me what materials are considered to be
biocompatible? PMMA (make solution 20 to 150 g/liter in Xylene, or other
high boiling point solvents)
                        Polycarbonate (benzene, Iso butyl acetate, xylene)

2. Parylene C is often reported to be one of them, and it is said to be
vapour deposited.  Does this mean, it is deposited by Chemical Vapour
Deposition?

3. Are the following biocompatible: glass (YES), silicone rubbers (YES, MOST
OF THEM), PMMA? (GENERALLY YES, DEPENDS ON ADDITIVES)


Thank you very much for your time.


Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
The Branford Group