RE: Pyralene C and Biocompatible materials needed
1999-03-23
Karl Cazzini
1999-03-24
Thor Osborn
1999-03-24
Dr. Mark W. Lund
1999-03-23
Karl Cazzini
1999-03-24
Dr. Mark W. Lund
RE: Pyralene C and Biocompatible materials needed
Dr. Mark W. Lund
1999-03-24
Dear Sung Jin,
Parylene C might be considered to be vacuum deposited.
The dimer is sublimed, then this gas is passed through
a furnace at 700 degrees C, where the dimer breaks down
into monomer molecules.  The monomer gas is then
passed into the coating chamber at room temperature.
Three monomers must come together to start the polymerization,
which is nearly impossible in the gas, but like ly on
surfaces, so the gas can penetrate into every nook and
cranny, then polymerize on the surface.  Thus it can
be made thin, conformal, and complete.  It is very intert
(I mean inert) and strong.

best regards
mark

Mark W. Lund, PhD
VP Engineering  >> Soft X-ray Web page http://www.moxtek.com<<
MOXTEK, Inc.
452 West 1260 North
Orem UT 84057       801-225-0930        FAX 801-221-1121
[email protected]

"This is a YOUNG business...How can I tell you what
YOUR job is when I don't know what MINE is?" --Pogo


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics