I read your message forwarded to me by a collegue, and look for helping you :

Find herafter 2 labs playing with such an ellipsometer in France :

B. DREVILLON
Laboratoire de Physique des Interfaces et des Couches Minces
Ecole Polytechnique
F 91128 PALAISEAU

Jean-Yves ROBIC
CEA/DLETI/CMO
17, rue des martyrs
F 38054 GRENOBLE CEDEX
Phone : (33)76.88.42.27
Fax : (33)76.88.50.46

Please, what MEMS stand for ? I am involved in pyroelectric imagers...

Regards.

G. Boucharlat
Thomson-CSF
BP 123
F 38521 SAINT EGREVE CEDEX
[email protected]
-------
Following is a forwarded message.
Original Sender :  ///FR/ATLAS/INTERNET////RFC-822:rizo(a)me.umn.edu
Original Subject: ELLIPSOMETER
Original TO :///FR/ATLAS/INTERNET////RFC-822:MEMS(a)ISI.EDU
Original Importance: NORMAL

-------



I am searching for institutions/companies that may
have an ellipsometer for directly measuring thin film
(metal and dielectric) optical constants (n and k)
in the region from 8 to 15 microns (i.e., 1250/cm
to 667/cm   or 3.75e13 Hz to 2.00e13 Hz   or
0.16eV to 0.083 eV).

My literature search to date has suggested that the
only such devices exist in Europe (France and Germany).

I would appreciate any leads on any such devices
either commercially available or "jerry-rigged" in
some lab.  The application is for a MEMS-related
pyroelectric detection system.


-thanks

Raed Rizq
"[email protected]"
University of Minnesota


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review
Tanner EDA by Mentor Graphics