Hi Fabio,

the dielectric constant of Pyrex is 4.6 (@1 MHz, 20deg. C)

Ralf

Fabio Coccetti schrieb:
>
> Hallo Everybody
>
> I would appreciate if someone could provide me with the value of Pyrex
> dielectric constant.
>
> Thanks in advance
>
> FABIO
>

--
**************************************************************
Dipl.-Ing. Ralf Keller
Fraunhofer-Institut Biomedizinische Technik
Ensheimer Str. 48
D-66386 St. Ingbert
Germany
Tel.:   +49 (0)6894 980-158
Fax:    +49 (0)6894 980-400
e-mail: [email protected]
web:    http://www.ibmt.fhg.de
--MimeMultipartBoundary--


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
Addison Engineering