Re: wet etching of Pt
Sony V. Lemoff
1999-04-07
Have you tried aqua regia to etch Platinum? Otherwise, you could get rid of
Pt by doing a lift-off process. Let me know if this helps.

-Sony Lemoff

>Dear All,
>I am urgently looking for an effect method (preferly wet) to etch electrode
>platinum (Pt) on silicon substrate with a thin layer of Ti. Would you please
>give me help?
>Best regards.
>
>________________________________________________________________
>Dr Kong Lingbing
>School of EEE
>Nanyang Technological University
>Block S1, Nanyang Avenue
>Singapore 639798
>
>Tel: (65) 7906084
>Fax: (65) 7933318
>Email: [email protected]
>________________________________________________________________
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics