I would recommend the following:

        Handbook of Semiconductor Silicon Technology
        By: Noyes Publications
        Edited By: William C. O'Mara, Robert B, Herring and Lee P. Hunt

Happy hunting!
Roger Neef
Silicon Valley Microelectronics, Inc.