MEMSnet Home: MEMS-Talk: Re: Si wafers
Re: Si wafers
1999-02-02
Kholdoun TORKI
Re: Si wafers
Kholdoun TORKI
1999-02-02
Dear Christophe,

SOI wafers can be obtained in small or large quantities from
SOITEC (Grenoble, France).
They have 4", 6", and 8" SOI wafers with different types
of substrate thickness.
We ordered in the past wafers in small quantity. The service
and prices were fine.

You can contact Mr. LINDHEIMER, or Mr. THIBAULT

SOITEC SA
Parc Technologique des Fontaines
38190 Bernin,  France
Phone: +33 4 76 92 75 00
Fax: +33 4 76 92 75 01
e-mail: [email protected]

Regards,

===================================================================
Dr. Kholdoun TORKI          |    CMP-TIMA  46, Av. Felix Viallet, |
[email protected]      |    38031 GRENOBLE, France.          |
[email protected]          |    http://tima-cmp.imag.fr          |
Tel : +33 4 76574763        |    Fax : +33 4 76473814             |
===================================================================


Christophe Gorecki wrote:

> Dear MEMS collegues:
> Can you tell me the commercial source of best quality/price Silcone
> wafers. I research 3 categories of wafer:
> 1. test wafers of 200~500 micron thick. Not specially flat but chip.
> 2. high quality flatness.
> 3. SOI wafers.
> The source can be in Europe (France ?) or US.
> Sincerely,
> Christophe Gorecki
>
> --
> *******************************************************************
> Dr. Christophe Gorecki, Senior Researcher
> Laboratoire d'Optique P.M. Duffieux,Universiti de Franche-Comti
> 16 Rte de Gray, 25030 Besangon Cedex, France
> Tel: +33-3-81666594, fax: 33-3-81666423
> e-mail: [email protected]
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.