What's the best surface roughness of HF or BOE etching of Pyrex glass? Under
what condition: temperature, HF concentration? What's the etch rate?

Where can I get plastic substrate for making micro-channels? Any references
of the processing on plastic substrate?

Thank you for your time and info.

Ying Xu
MEMS Applications Engineer
phone: (626)-685-5930
fax: (626)-432-5705


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
University Wafer
Addison Engineering