forming feather edges / burrs in metals
1999-04-23
Karl Cazzini
forming feather edges / burrs in metals
Karl Cazzini
1999-04-23
I am trying to form, good quality, homogeneous feather edges (or burrs) on
thin metal strips (0.006" thick), by grinding and / or polishing methods. I
realise that most peolple want to eliminate these "burrs" or feather edges,
however I actually require them! I am grinding stainless steel strips (~1
inch long, 0.006" thick) at angle of about 15 degrees, on a rotating
abrasive disk. If the abrasive is too course, a poor quality, inhomogeneous
feather edge results. I want to form good quality, homogeneous and
REPRODUCEABLE feather edges in SS, for a MEMS application that I am working
on. Any and all assistance would be most welcome. Please remember that this
is something I must be able to do in-house. I do have access to quality
polishing and grinding equipment. Any assistance would be greatly
appreciated. Thanks very much, Karl.


******************************
* Karl H. Cazzini (Ph.D)     *
* Conifer Group & Associates *
* 116 Cochituate Road        *
* Framingham MA 01701        *
* USA                        *
*                            *
* Tel(W): (508) 620 8845     *
* Fax(W): (508) 620 8830     *
* Tel(H): (508) 875 2009     *
******************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
MEMStaff Inc.
University Wafer