Nakash:

Yes we at Norsam Technologies have been building sub-micro cantilevers
in Silicon, Nitide and metal substrates using Focused Ion Beam Enhanced
Etching technique for thin film stress measurement and other
applications. We do provide services in this area and if you need more
information on this please call me at 503-640-0586 or send me an email.
Thank you

Regards
Jayant
*****************************************
Jayant Neogi
Vice President & Chief Technical Officer
Ph#  503-640-0586
Fax  503-640-8117
http://www.norsam.com
*****************************************
Nakash Ronen wrote:
>

> Dear collegues ,
>         Does any of you have information about micro Aluminum
> (or other metal) cantilevers manufacturing technique ?
> Any help or source of information will be gratefully accepted .
> My E-Mail is : [email protected]
>
>         Thanks ,
>                  Ronny N.
>
>

--


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
The Branford Group
Addison Engineering