Carlos Mastrangelo
1999-04-21
              polysilicon



It is 2.3 gr/cm^3. Same as for bulk.


On Mon, 19 Apr 1999, Dung-An Wang wrote:

> Dear MEMS people
> Could you tell me what the density of LPCVD polysilicon is ?
> I much appreciate that.
> Have a good day.
>
>
>
>    Sincerely,
>           Dung-An
>
> Phone:
>  Office: (734) 615-0303   Home  : (734) 662-1553
> Address:
>  Office:                               Home:
>   University of Michigan                  411 Longshore Dr.
>   Department of Mechanical Engineering    Ann Arbor, MI 48105
>   3007 EECS, 2350 Hayward                 U.S.A.
>   Ann Arbor, MI 48109-2125
>   U.S.A.
> E-Mail:
>    [email protected]
> Homepage:
>    http://www-personal.engin.umich.edu/~wangd
>
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Addison Engineering
Nano-Master, Inc.