A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Silver As Si Etch Mask
Re: Silver As Si Etch Mask
1999-04-22
[email protected]
1999-04-22
Albert K. Henning
1999-04-27
Jonathan Bernstein
Re: Silver As Si Etch Mask
[email protected]
1999-04-22
Dear Mark,

I would recommend consulting the "CRC handbook of metal etchants" by Perrin
Walker and William H. Tarn. You will be amazed at the options it will provide
you. I don't have a copy, otherwise I would give you the options for silver.

Regards,
Mike Mattes