Hello everybody,
      Do you have any method about drilling small holes on SiO2 glass? The
diameter of the hole is less then 1mm, and the depth is 500um, the same as
the thickness of glass. It will spend long time, if wet-etching is used,
maybe 1 month. I do not know if mechanical method is OK.
     Thanks a lot.

*************************************
Kai Sun( $BB9!!3. (J)
Dept. of EcoSystem Engineering,
Graduate School of Engineering,
The University of Tokushima,
2-1 Minamijyosanjima,
Tokushima 770-8506, Japan
Tel: 4378 (O)
*************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.