Dear MEMS researchers,

We would like to laminate the magnetic core of microtransformers by
electroplating insulating material between each layer of magnetic
material.

Does anyone have any information on electroplating thin layers (less
than 5 microns) of conductive polymers and/or on how to make this layer
insulating by a post treatment.

Thanks a lot

Magali Brunet, PhD.
NMRC,  Cork, Ireland
tel:+353-21-90-42-79
e-mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review
Addison Engineering