Three sources of MEMS-related fabrication information include:

 1. S.M. Sze (ed.), Semiconductor Sensors, John Wiley and Sons, Inc., NY, NY,
    1994 (especially Chapter 2 and the references at the end of the chapter).
 2. Julian W. Gardner, Microsensors - Principles and Applications, John Wiley
    and Sons, 1994 (especially Chapter 3 and the references at the end of the
    chapter).
 3. C.D. Fung, P.W. Cheung, W.H. Ko and D.C. Fleming (eds.), Micromachining and
    Micropackaging of Transducers, Elsevier, Amsterdam, 1985 (especially the
    chapter by W.H. Ko, J.T. Suminto and G.H. Yeh, "Bonding Techniques for
    Microsensors," pp. 41-62).

Best regards,

Ed Kolesar


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Addison Engineering
Harrick Plasma, Inc.