A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RIE etching of YAG
RIE etching of YAG
2000-06-09
Keith Jackson
RIE etching of YAG
Keith Jackson
2000-06-09
To group
I was asked to look into the possible RIE etching of YAG ( Yttrium Aluminum
Garnet). I wish to use RIE to etch a circular or square mesh pattern either
3 um in diameter or 3um on a side in the case of a square mesh. The etch
depth in the YAG should be 3um. Any suggestions, leads, or ideas would be
appreicated.
--
Keith Jackson
Lawrence Berkeley National Laboratory
Berkeley,Ca 94720
510-486-6894 voice
510-486-4955 fax


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMStaff Inc.
Mentor Graphics Corporation