Hi everybody,

My problem is to build membranes made of polyimide material.
Contrary to usual applications of polyimides, we do not want to deposite
them on a substrate. What we want is to build membranes (surrounded by
air on the both surface) of one to few thousands angstroms thickness.
They will be attached to a ring used as a support for the membranes.
This ring will be typically of two centimeters large.

We would like to use polyimides because of  their particularly good
mechanical properties.

Do you know if it is possible to use those products ? Which one ? What
is the method to apply ?

Thanks a lot

Stephan Thiberge
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
University Wafer
MEMS Technology Review