MEMSnet Home: MEMS-Talk: RE: Selective Wafer Bonding
RE: Selective Wafer Bonding
2000-01-05
Mirza Andy
RE: Selective Wafer Bonding
Mirza Andy
2000-01-05
Dear Weng On,

I assume that you cannot pattern (etch) one of the wafers so that only
certain surface regions of the wafer are available for bonding. In that
case, for silicon direct/fusion bonding there have been some reports of
selectively roughening wafer surfaces to limit bonding in those areas.

Please contact me directly for more information and to discuss your
application in greater detail.

Regards,
Andy Mirza
Technology Manager
Electronic Visions, Inc.
3701 E. University Drive
Ste. 300
Phoenix, AZ 85034
Tel: (602) 437-9492
Fax: (602) 437-9435
E-mail: [email protected]
Web: http://www.elvisions.com

=============================================



-----Original Message-----
From: choong weng on [mailto:[email protected]]
Sent: Tuesday, December 28, 1999 1:03 AM
To: Mirza Andy; [email protected]; [email protected]
Subject: Selective Wafer Bonding


Dear All,

  I need to bond two wafers but selectively at certain
locations only.  Please provide me any information
with regards to selective wafer-wafer bonding?  Thank
you very much.

Weng On



=====
Best Regards,
Yongan
__________________________________________________
Do You Yahoo!?
Talk to your friends online with Yahoo! Messenger.
http://messenger.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
MEMStaff Inc.