Dear all,

  I am looking for advice and comments on how to carry
out multiple layer anodic bonding between silicon and
borosilicate glass wafers.

  Secondly, what are the methods I can use to drill
holes (in the order of 1mm dia) in borosilicate glass.
 Thank you very much.


CHOONG Weng On
National University of Singapore

=====

Best Regards,

CHOONG Weng On
MEMS-LAB (EA 02-09)
National University of Singapore
DID: +65 874-4567
Fax: +65 874-4509

__________________________________________________ Do You Yahoo!? Kick off your party with Yahoo! Invites. http://invites.yahoo.com/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group