What's the depth of the holes? Your PR thickness should be at least a half
of the depth of the hole. Try to spin a viscous PR.

Yahong

>From: SILLON Nicolas 
>Reply-To: SILLON Nicolas , [email protected]
>To: [email protected]
>Subject: Photoresist deposit on KOH holes
>Date: Fri, 4 Aug 2000 08:39:27 +0200
>
>Hi,
>
>I need to deposit photoresist on a wafer with KOH holes. With standard
>methods I am not able to cover correctly the edges of the holes.
>Does anybody can help me?
>
>Thanks.
>
>Nicolas.
>
>
>
>

________________________________________________________________________
Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Nano-Master, Inc.
MEMS Technology Review