 **Cool grease can be purchased from AI Technology Inc, 9 Princess Road,
> Lawrenceville, NJ 08648 (email [email protected]).

Cheers,
Greg Ortiz
Surface Technology Systems
West Coast Regional Sales Manager
611 Veterans Blvd, #107
Redwood City, CA 94063
Phone 650 569 3655 x16
Pager 1 800 713 9841
Cell 408 499 5689
Fax 650 569 3663

----------
> From: [email protected]
> To: [email protected]
> Subject: Cool grease vendor
> Date: Monday, August 14, 2000 6:45 PM
>
> Hello,
>
> I am trying to get a hold of something called "cool grease" It can be
used for attaching backing wafers during deep RIE etching. I have been told
that it works better than photoresist because it has greater thermal
conductivity.
>
> Does anyone know of a vendor for this product?
>
> Thanks,
> Shivalik
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
The Branford Group