Hi,

We are trying to electroplate Indium to make
solder bumpers for wafer bonding. However,
the surface of the plated Indium turned out to
be very rough, although the current density
we used is low. The plating bath is ready
to use and no other solutions need to be
added. Also we've checked the pH value of
the solution. It is ok too.

Anyone has the experience of Indium plating
before? Could you please give us any suggestion?
Thanks very much!

Xyuan

__________________________________________________
Do You Yahoo!?
Yahoo! Messenger - Talk while you surf!  It's FREE.
http://im.yahoo.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Mentor Graphics Corporation
MEMS Technology Review