Mechanical properties of Si chips.
1996-04-15
HaKAN ELDERSTIG -1080
Mechanical properties of Si chips.
HaKAN ELDERSTIG -1080
1996-04-15
Silicon is a strong material they say....

We have put our bulk micromachined silicon chips in a plastic package. Some of
the chips breaks or we can se fine cracks, usually close to the v-grooves.
There is a bonded glass lid on top of the v-grooves that should strengthen the
device. The chips also had been edge polished after dicing with 3 microns and
0.3 micron papers. Do anyone know if the polishing itself can lower the
mechanical strength of the chips? Or is the dicing bad enough?

Hakan Elderstig


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer