MEMSnet Home: MEMS-Talk: RE: Anodic bonding of alloy "39" to 7740
RE: Anodic bonding of alloy "39" to 7740
2000-01-21
Mirza Andy
RE: Anodic bonding of alloy "39" to 7740
Mirza Andy
2000-01-21
Dear Mike Barton,

A variety of metals and alloys have been anodically bonded to Pyrex (Corning
#7740). I'm not familiar with all the details for alloy "39", but the
following are some of the materials you might consider for your application:
aluminium, titanium, tantalum, chromium, Kovar, Niromet 44 and Fe-Ni-Co
alloy.

Please feel to contact me if you have any questions on anodic bonding, as we
have some experience with this bonding technology.

Regards,
Andy Mirza
Technology Manager
Electronic Visions, Inc.
3701 E. University Drive
Ste. 300
Phoenix, AZ 85034
Tel: (602) 437-9492
Fax: (602) 437-9435
E-mail: [email protected]
Web: http://www.elvisions.com

=====================================

-----Original Message-----
From: Mike Barton [mailto:[email protected]]
Sent: Thursday, December 30, 1999 10:05 AM
To: [email protected]
Subject: Anodic bonding of alloy "39" to 7740


We have tried, unsuccessfully, to anodicaly bond alloy "39" to
borosilicate (7740).  Does anyone know what the basic process parameters
are?  Should we try different alloys? Any help on this would be greatly
appreciated.

Thanks,
Mike Barton
Creare, Inc.
Etna Rd, PO Box 71
Hanover, NH 03755
Phn (603) 643-3800
fax (603) 643-4657
email [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
MEMStaff Inc.