I am looking for information on bonding or sealing of glass to glass. The glass
parts come in the form of polished flat substrates, and can be as thin as
microscope slides or as thick as photomask blanks (0.90 inch). The bond should
be direct--I would like to avoid using bonding films or adhesives. However,
glass-based bonding layers which can be deposited on one or both of the glass
substrates would be alright. The bonding can be done at any temperature
provided the glass parts are not deformed or distorted. The glass can be any of
the commonly available commercial glasses such as soda-lime, borosilicate, or
even fused silica. I would appreciate any information or leads.

Thanks,

Alex Shimkunas
Nanostructures, Inc.
3070 Lawrence Expy
Santa Clara, CA 95051
(408) 733-4345
Fax (408) 733-4347


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group