Mr. Westra,

AZ offers a thick resist, part # AZ P4620. The resist thickness is from about 5
to 10 microns, depending on spinning rpm. You will probably have to apply two
or three layers to satisfy your 20 micron thickness requirement.

AZ Photoresist Products is a subsidiary of Hoechst Celanese Corp.,
headquartered in Somerville, New Jersey. The phone # there is (908) 429-3500,
or you might also try (800) 515-4164.

Charles King
Research Assistant-UCLA Electrical Engineering Dept.
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Tanner EDA by Mentor Graphics