Dear colleagues

By accident, our team  came up with an exciting development of a new
MEMS process for  fabrication a large area, free standing ultra-thin
membranes (typical size 10-20  mmsqr, 5-20 nanometer thick!). These
composite membranes are surprisingly robust.

I am looking for potentials application, I will be happy to discuss them
with someone, particularly in the field of uncooled IR detectors and
MOEMS.

Thank you for any help you can offer.

Jovan Matovic


----------------------------------------------------------------------
Jovan MATOVIC                           |Tel: (++381) 11 630 - 757
University of Belgrade,IHTM - CMTM      |Fax: (++381) 11 182 - 995
Njegoseva 12,11000 Beograd, Yugoslavia  |email: [email protected]
TU - Wien, Austria
Institut fur Feinwerktechnik
_______________________________________________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group