hi! I am working in the Microelectronics Centre of IIT Kharagpur, India,
in a project where we are developing a Micromachined Flowsensor. I need
help regarding nickel thin film deposition on silicon dioxide.If any
body has any data in this regard please kindly help me.We are using a
1.0 micron thick SiO2 layer to deposit nickel.Please kindly send data
regarding nickel adhesion quality on silicon dioxde and what type of
filament and which metal filament can we use.
Thanks With Regards,
Kanishka Biswas

------------------------------------------------------------------------
Get your FREE download of MSN Explorer at http://explorer.msn.com[1]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
MEMS Technology Review