Hi,

Can anybody provide me with detail information on chemical etchants
efficient in patterning of PZT thin films (deposition by sol gel on Si
substrate +Pt/Ti electrodes, thickness < 1µm) or let me know where can I
obtain such informations on the website.
Thank you in advance !
Best regards,
Christophe Gorecki
  *******************************************************************
Dr. Christophe Gorecki, CNRS Senior Researcher
Laboratoire d'Optique P.M. Duffieux, Faculte des Sciences et Techniques
16 route de Gray, 25030 Besancon, France
Tel: +33-3-81666607, fax: +33-3-81666423
e-mail: [email protected]




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
University Wafer
Nano-Master, Inc.